Material Cast Iron Drawing No. -
Stage After Casting Surface Condition As Cast
Technique Direct Visual Inspection
Test Devices Used
Surface Preparation
Lighting Equipment
Light Intensity 1200 Lux Meter -
Part Surface Temperature 35 °C Thermometer
Examination Extent 100% (Accessible Area Only)
Specification/Standard/Procedure ASME SEC V Edn 2021
Acceptance Standard  ASME Sec VIII Div.1 App. 8
OBSERVATION AND RESULTS
Sr. No. Description Qty
1 Heat No. 1357 1
2 Tag No. 2468 1
Imperfections
Imperfection Type Observations / Evaluations Imperfection Type Observations / Evaluations
Hot Tears and Cracks No Wrinkles, Laps, Folds & Cold shuts No
Shrinkage No Cutting marks No
Sand Inclusions No Scabs No
Gas Porosity No Chaplets No
Veining No Weld Repair Area No
Rat Tails No Surface Roughness No

Remark:

Note:

 
ID - 5451 VISUAL EXAMINATION REPORT REQ ID - 23-24/130
Client Auto Mech (India) Pvt. Ltd, Pune Report No. IBTS/VT/23-24/130
Address Gat No.216. Santoshnagar (Waki). Tal. Khed, Dist. Pune Revision 2
Report Date 02-Aug-2025
Component Visual inspection of castings Test Date 01-Jan-2025
Supplier